Electrodeposition of nanocrystalline Ni-Mo alloys from alkaline glycinate solutions
(
Electrochemical Science Group
, 2014 , Article)
The induced electrodeposition of nanocrystalline Ni-Mo alloys was investigated using two different molar ratios of Ni:Mo in sodium glycinate solution at pH 9.3. The chemical nature of the Ni2+ and MoO4 2- in alkaline ...
Electrodeposition of 70-30 Cu-Ni nanocomposite coatings for enhanced mechanical and corrosion properties
(
Elsevier
, 2016 , Article)
A copper-nickel alloy (70:30 ratio) was electrochemically deposited and compared to a composite coating incorporating layered silicate platelets to obtain copper-nickel-montmorillonite (MMT). The composite coatings were ...
Salt water corrosion resistance of electrodeposited Ni-layered silicate nanocomposite coatings from Watts' type solution
(
Elsevier B.V.
, 2014 , Article)